ZL104 Al-Si-Mg-Ti Gravity Cast Gearbox Housings and Bearing Carriers

Drawing-based ZL104 Al-Si-Mg-Ti gravity cast gearbox housings with chemistry, porosity, heat-treatment, machining, leak and RFQ controls.

Category:

Description

EB Castworld accepts drawing-based RFQs for ZL104 Al-Si-Mg-Ti gravity cast gearbox housings and bearing carriers. Candidate parts include split housings, covers, motor/gear adapters, bearing-support frames and oil-containing enclosures. Tooling, gravity permanent-mould or other approved casting route, heat treatment, machining and leak testing are reviewed from the actual drawing and order quantity.

ZL104 is a Chinese cast-aluminum alloy designation controlled by the adopted GB/T 1173 edition. It is not automatically identical to A356 or another international grade. Cross-standard substitution requires written comparison of chemistry, temper, product form, mechanical properties, casting route and testing. No stock, price, delivery time, load rating or leak performance is inferred from the alloy name.

Silicon, magnesium and titanium are important to castability, strengthening and structure, but iron, copper, manganese, zinc and other residuals also need control. Geometry, hydrogen/oxide management, feeding, solidification, heat treatment and machining can be as important as the melt certificate.

Product scope and drawing-based quotation boundary

This page targets purchasing intent for a ZL104 gearbox or bearing housing made to customer drawings. It is separate from the site’s generic ZL104 casting page, compressor-casing Blog and A356/ZL101/ZL104 pump-housing product. The component, pressure/leak boundary and acceptance evidence are different.

Provide gear and bearing loads, shaft alignment, mounting condition, lubricant, temperature, vibration, sealing system and assembly sequence. EB Castworld reviews manufacturability; the gearbox OEM retains structural, bearing, thermal, noise/vibration and lubrication design.

Candidate component Drawing inputs Service inputs Engineering boundary
Split gearbox housing Split face, bores, dowels, feet, cover and oil passages Torque, alignment, lubricant, temperature and vibration OEM approves stiffness, gear mesh and bearing life.
Bearing carrier/end cover Bore, flange, seal land, bolt circle and runout Bearing load, speed, fit and lubrication Fits require assembly-system approval.
Motor/gear adapter Pilot, concentricity, face runout and mounting pattern Torque, thermal growth and alignment Casting does not approve drive-system dynamics.
Oil-containing enclosure Wall, drain/fill, seals, threads and joint face Fluid, temperature and leak-test requirement Leak test does not establish pressure-vessel design.

GB/T 1173 ZL104 material identity and casting-route limits

China’s national standards platform lists GB/T 1173-2013, Casting aluminium alloy, as current, last reviewed in August 2025 with a revision project in progress. The purchase order must state the edition actually adopted; a future revision cannot be silently applied. Chemistry and delivery condition should be taken from the controlled standard text, not a secondary web table.

ASTM B108/B108M-25 covers aluminum-alloy permanent-mould castings and ASTM B26/B26M-25 covers sand castings under their own alloy systems. They help establish process/product-form boundaries but do not turn ZL104 into an ASTM grade. ISO 8062-3:2023 may frame general casting tolerances and machining allowances when invoked on the drawing.

Reference or designation What it controls What it does not prove RFQ action
GB/T 1173-2013 ZL104 Chinese cast-aluminum alloy identity and chemistry Finished housing load or leak performance State edition, condition and tests.
ASTM B108/B108M-25 Permanent-mould castings in its listed alloy system Automatic ZL104 equivalence Use only when contractually applicable.
ASTM B26/B26M-25 General-purpose sand-cast alloy requirements Highly loaded/safety-critical integrity by itself Add drawing-specific properties and NDT.
ISO 8062-3:2023 General casting tolerance/allowance framework Bearing-bore or split-face CTQ Individually tolerance functional features.

Al-Si-Mg-Ti chemistry, iron control and residual elements

The order should request actual heat analysis for every element controlled by GB/T 1173 and any customer residual limits. This page intentionally avoids publishing a simplified universal range: only the adopted standard and purchase specification control release. Spectrometer results must remain linked to melt, pour lot and castings.

Silicon supports fluidity and castability; magnesium contributes to precipitation-strengthening response when the specified heat treatment is applied; titanium may participate in grain refinement; iron can form intermetallics that affect ductility and machining; copper, manganese, zinc and other residuals can alter properties and corrosion. Al is the balance, not evidence of purity or soundness.

Element or group Metallurgical role Procurement evidence Important limit
Silicon Fluidity, solidification and Al-Si structure Actual heat value and approved alloy Si cannot prevent oxide films or shrinkage.
Magnesium Heat-treatment/strengthening response Actual analysis plus thermal record Mg alone does not prove temper or core properties.
Titanium/grain refiners Nucleation and structure control when approved Addition practice and chemistry Excess or fade effects require process control.
Iron/intermetallics Ductility, machining and fatigue considerations Specified maximum and process evidence A passing bulk value does not show morphology.
Cu, Mn, Zn/residuals Corrosion, phase and property balance Complete certificate Do not release from Si/Mg values alone.

How the element system connects to component duty

Chemistry must be interpreted with melt cleanliness, hydrogen control, oxide management, solidification rate and heat treatment. A tensile bar cast separately from the housing may not represent a thick bearing boss or thin wall. The purchaser should define coupon type and whether casting properties are required.

ZL104-to-A356 comparisons are often used for orientation, but nominal similarity is not contractual equivalence. Differences in residuals, modification, temper, standards and property scope require engineering review before substitution or shared tooling assumptions.

Element/process interaction Useful engineering question Unsafe shortcut Required control
Si + mould fill Can thin walls and ribs fill without cold shuts? Raising temperature without oxide control Simulation/trials and controlled pour window.
Mg + heat treatment Will the specified temper produce required properties? Approving from chemistry only Furnace/quench/age record and tests.
Fe + section/structure Could intermetallic morphology reduce ductility? Using one hardness number as proof Chemistry, process and representative evidence.
Hydrogen + oxides Are porosity and films controlled in pressure/leak zones? Relying on impregnation as routine cure Melt treatment, handling and agreed inspection.

Bearing bores, split faces, ribs, bosses and oil-tight walls

Gearbox housings combine thin walls, ribs, heavy bearing bosses, mounting feet and machined split faces. Abrupt sections can create feeding hot spots and distortion. The drawing should define minimum wall, radii, draft responsibility, machining pads, core locations and prohibited-repair zones.

Bearing-bore alignment depends on a stable datum and machining in the correct assembled condition. If split halves are line-bored together, specify matched marking, fasteners/dowels and inspection assembly. Seal grooves, drains and threaded ports need wall and positional control.

Critical feature Why it matters Drawing or inspection requirement Failure prevented
Bearing bore Alignment, fit and bearing temperature Diameter, coaxiality, roundness, finish and assembled condition Noise, heat and premature bearing damage.
Split/joint face Sealing and structural closure Flatness, dowels, bolt pattern and finish Oil leak and bore distortion.
Boss/rib transition Load transfer and casting feed Radius, section, location and NDT zone Hot spot and fatigue crack.
Oil wall/port Containment and service access Minimum wall, threads, plugs and leak boundary Porosity leak and stripped thread.
Aluminum housing casting for ZL104 geometry and bearing bore review
Existing EB Castworld media-library photograph used as generic aluminum-casting context. Exact alloy, heat, customer and project provenance was not independently re-established; appearance does not prove ZL104 chemistry, temper or gearbox approval.

Gravity casting, permanent moulds, cores and melt-quality control

Gravity permanent-mould casting can offer repeatability and useful surface/dimensional control for suitable housing geometry and volume. Steel inserts, sand cores or alternate routes may be considered only after review. Mould temperature, coating, fill path, venting, feeders and controlled solidification affect oxide entrainment, cold shuts, shrinkage and distortion.

Charge material, returns, degassing, fluxes, grain refinement/modification and holding time require written controls. A clean spectrometer result does not prove low hydrogen or absence of oxide films. Tooling and first articles should be validated before production release.

Manufacturing stage Risk to manage Required control Record
Charge/melt treatment Residuals, hydrogen, inclusions and fade Approved charge and treatment window Heat and treatment log.
Mould/core Temperature, shift, gas and surface defects Tooling, coating, vent and core plan First-article record.
Fill/feed/solidify Oxide folds, cold shut, shrinkage and hot spot Gating/feeding and process window Pour-lot traceability.
Trim/straighten Cracks, lost stock and distortion Approved trim, deburr and correction Visual/dimensional record.

Solution treatment, quenching, ageing and dimensional stability

Use only the heat-treatment condition ordered for ZL104 and the component. Solution treatment, quench transfer, water temperature/agitation, ageing and furnace loading can affect strength, residual stress and distortion. A T6 label without actual process and tests is insufficient.

Bearing bosses, ribs and thin walls respond differently to quenching. Fixtures and machining sequence should anticipate distortion. Stress relief or artificial ageing changes require purchaser approval because they can change both properties and dimensions.

Section thickness and test-piece representation

Define whether mechanical tests come from separately cast bars, attached coupons or the casting. Their cooling and thermal histories differ. If housing-wall properties or hardness maps are critical, state the exact location and method. Do not apply a small standard-bar value automatically to every heavy boss.

Line boring, split-face machining, threads and leak-test preparation

Establish cast datums before removing stock and retain identity through matched halves. Rough machining can reveal porosity; add a hold point before final line boring. Control cutting forces and clamping so thin walls are not distorted into an apparently acceptable bore.

Thread inserts, plugs, impregnation, weld repair and local peening are not assumed. If allowed, define procedure, zones, qualification and reinspection. Leak testing should occur in the assembly condition and after operations capable of opening a leak path.

  • Define rough/final stock and cast datum targets.
  • State matched-half, dowel and line-boring condition.
  • Control bores, split face, seal lands, feet and shaft-center distances.
  • Inspect threads, inserts, drains and plugs.
  • Reinspect exposed surfaces after rough machining.
  • Define cleaning and leak-test preparation.
Aluminum casting illustrating machining porosity and leak inspection planning
Existing EB Castworld media-library photograph used as general machining context. Exact material, drawing and inspection provenance was not independently re-established; the image does not prove GB/T 1173 conformity or a passed leak test.

Inspection, NDT and quality-document package

Inspection should cover heat identity, chemistry, dimensions, visual workmanship and the specific integrity risks of the housing. Radiography or CT may be specified in bearing bosses or oil walls; penetrant can address selected surface openings; leak testing checks the assembled boundary under defined conditions. Acceptance zones and methods must be stated.

The dossier should link melt/pour lot, heat treatment, repairs, dimensions and test results. Sampling plans must reflect critical characteristics. AQL sampling is not appropriate for a characteristic whose escape is unacceptable unless the responsible purchaser explicitly defines it.

Inspection layer Purpose RFQ definition Method boundary
Chemistry/traceability ZL104 identity GB/T edition, actual values and pour-lot marking Does not prove porosity or temper.
Dimensions Assembly and alignment Datums, assembled condition, CMM/gauges and CTQs Clamping can mask distortion.
RT/CT or PT Selected internal/surface discontinuities Zones, sensitivity, timing and acceptance No method proves absolute defect freedom.
Mechanical/hardness Heat-treatment consistency Specimen source, condition and limits Separate bars may not represent bosses.
Leak test Defined oil/air boundary Medium, pressure, time, temperature and leak limit Does not approve structural load or service life.

Oil leakage, bore distortion, boss cracking and bearing misalignment

Preserve the leak path, assembly condition and operating data before repair. Record torque, dowel/fastener condition, bearing temperatures, vibration, oil, thermal cycles and prior sealant or impregnation. A visible pore may be one contributor rather than the root cause.

Use dimensional mapping, pressure/leak localization, metallography and process records to distinguish shrinkage, gas porosity, oxide film, machining exposure, thread damage or structural cracking. Do not authorize a weld or larger insert before checking remaining wall and heat-treatment implications.

Observed problem Possible contributors Evidence before changing material Corrective-action boundary
Split-face leak Flatness, clamping, seal, porosity or crack Assembled flatness, bolt/dowel, pressure map OEM approves sealing/design changes.
Bore misalignment Distortion, clamping, heat treatment or machining datum Free/assembled dimensions and process history Remachining must preserve wall and center distance.
Boss crack Stress concentration, shrinkage, load or repair Origin, section, loads and NDT Material substitution alone may not solve geometry.
Thread pullout Wall, engagement, torque, porosity or insert Drawing, torque and local section Insert repair needs written approval.

First-article and production-release checklist

  1. Approve drawing, CTQs and tooling responsibility.
  2. Confirm GB/T 1173 edition and ZL104 condition.
  3. Review charge, melt treatment, mould/core and fill plan.
  4. Link pour lot to chemistry and castings.
  5. Complete ordered heat treatment and tests.
  6. Inspect first-article walls, bosses, bores and split faces.
  7. Perform specified RT/CT/PT at defined stages.
  8. Machine matched features in the approved assembly condition.
  9. Complete leak test and dimensional dossier.
  10. Release deviations only through purchaser approval.
Aluminum cast component for ZL104 traceability and dimensional inspection
Existing EB Castworld media-library photograph used as generic casting context. Exact grade, melt, customer and service provenance was not independently re-established; it is not represented as a verified gearbox customer project.

RFQ checklist for a ZL104 gearbox housing

  1. 2D drawing and 3D model with revision and datums.
  2. Gearbox duty, loads, speed, alignment, temperature and vibration.
  3. Lubricant, sealing system, leak boundary and cleaning.
  4. ZL104 material standard/edition, condition and substitution policy.
  5. Chemistry, residuals, melt treatment and traceability.
  6. Gravity mould/core route, wall minima, draft and repair zones.
  7. Heat treatment, coupon source and mechanical/hardness requirements.
  8. Bores, split face, dowels, feet, threads, finish and line-boring condition.
  9. RT/CT/PT, dimensions, leak test and acceptance criteria.
  10. Tooling quantity, MTC, marking, records, packing and destination.

Related products, material guides and factory resources

Existing ZL104 casting product. ZL104 compressor-casing guide. A356/ZL101/ZL104 pump housings. Aluminum alloy composition guide. Materials. Engineering Resources. Quality Assurance. Factory Capability. Send Drawings for Quote.

This page targets a ZL104 gearbox-housing RFQ. The existing generic ZL104 casting, compressor-casing information and Al-Si-Mg pump-housing product retain separate product/application intent; none is presented as automatic interchangeability.

Current authoritative references

Engineering, commercial and safety boundary

This page is a drawing-based manufacturing and RFQ entry, not a stock offer or an equipment-design approval. The purchaser, equipment OEM and responsible engineer retain final responsibility for material selection, chemistry limits, product form, load cases, corrosion and wear compatibility, dimensions, heat treatment, machining, joining, inspection, installation, maintenance and retirement criteria. EB Castworld does not promise stock, price, lead time, service life, savings, certification scope or universal performance from a grade name, chemical element or website table. Final material, structure, thickness, dimensions, tolerances and installation method must follow the customer-approved drawing and contract.

Melting, forging, casting, heat treatment, machining, grinding, NDT, pressure or load testing and heavy lifting involve hot metal, rotating equipment, dust, fumes, chemicals, radiation sources and stored energy. Qualified personnel, applicable law, approved procedures, machine guarding, ventilation, PPE, calibrated equipment and exclusion zones remain required. Images on this page are existing site-library process context; their exact grade, heat, customer and project provenance was not independently re-established and they do not prove conformity of a future order.