Description
EB Castworld accepts drawing-based enquiries for QT500-7 C-Si-Mn-Mg ductile iron gearbox bearing housings, including split housings, pillow-block-style supports, bearing carriers, gearbox end covers and machined support brackets. Feasibility is reviewed from the controlled drawing, casting mass, wall transitions, bearing and seal interfaces, duty, annual quantity and required quality dossier.
QT500-7 is a Chinese spheroidal-graphite cast-iron designation. It should not be replaced by EN-GJS-500-7, ASTM A536 80-55-06 or another familiar label without a written comparison of the governing editions, test-piece rules, section sensitivity, matrix, hardness and supplementary requirements. A similar nominal tensile class does not create automatic equivalence.
The page emphasizes carbon, silicon, manganese and residual magnesium because their interaction influences graphite formation and matrix development. It does not publish one universal ladle recipe. Actual chemistry limits, nodularity criteria, matrix, mechanical properties and inspection acceptance must come from the adopted specification and customer-approved control plan.
Product scope and purchasing intent
The intended buyer has a housing drawing and bearing arrangement, or an OEM-authorized replacement definition. The RFQ should identify whether the supply is as-cast, rough-machined, finish-machined, painted or assembled with customer-approved inserts. Split-line relationship, line-bore condition and measurement under free or clamped assembly must be explicit.
A used housing is not automatically a master. Fretting, bore growth, cap distortion, paint thickness and field welding can change measured geometry. Reverse engineering therefore needs an agreed datum strategy, mating-component information and engineering disposition of damage before a model is frozen.
| Candidate supply | Required definition | Key risk | Approval boundary |
|---|---|---|---|
| One-piece gearbox housing | 3D model, bore centers, feet, covers and oil passages | Distortion and core shift | OEM approves stiffness, alignment and lubrication |
| Split bearing housing | Matched cap/base, dowels, bolt preload and line-bore state | Bore shift after assembly | Drawing defines measurement condition |
| Bearing carrier/end cover | Register, seal bore, flange and fasteners | Leakage and concentricity | Seal and bearing supplier data control |
| Legacy replacement | Authorized dimensions and damage disposition | Copying worn geometry | Purchaser approves recovered definition |
QT500-7, ISO 1083 and ASTM A536 boundaries
ISO 1083:2018 classifies spheroidal-graphite cast irons using mechanical properties measured on machined test pieces prepared from cast samples. ASTM A536-26 covers ductile iron castings and expressly notes that a precise quantitative relationship cannot be stated between properties at different casting locations or between a casting and its test specimen. Those cautions matter in a thick bearing boss connected to a thinner housing wall.
The purchase order should cite the controlling Chinese standard and edition for QT500-7, then separately define any ISO, EN or ASTM test method used. Cross-standard references are engineering tools; they do not convert one grade into another. If the buyer permits alternatives, the equivalence matrix and approval authority should be documented before quotation.
| Reference | Useful role | What it does not establish | RFQ instruction |
|---|---|---|---|
| QT500-7 | Ordered Chinese grade when tied to the stated standard | Automatic EN/ASTM equivalence | State standard, edition and delivery condition |
| ISO 1083:2018 | International classification of spheroidal graphite iron | A housing design or local-property guarantee | State grade and cast-sample method |
| ASTM A536-26 | Ductile iron casting specification and optional supplementary controls | A QT500-7 conversion table | Invoke only when contractually adopted |
| ISO 945-1 | Graphite-particle classification framework | Mechanical acceptance by itself | Define sampling, magnification and criteria |
C-Si-Mn-Mg chemistry, residuals and nodularization
Carbon and silicon establish the graphitization and matrix context; magnesium treatment promotes spheroidal graphite, while sulfur and oxygen affect treatment recovery. Manganese, phosphorus and carbide-promoting residuals can alter matrix and local properties. The actual workable window depends on charge materials, section size, inoculation, pouring temperature and specified matrix.
Request actual heat or ladle analysis for the elements controlled by the adopted grade plus purchaser residual limits. A single spectrometer result is not evidence of magnesium fade control, nodularity throughout the casting or a ferrite/pearlite ratio at every bearing boss. Traceability should link analysis, treatment lot, pour time and casting identity.
| Element/group | Metallurgical relevance | Evidence to request | Selection boundary |
|---|---|---|---|
| Carbon + silicon | Graphitization, fluidity and matrix balance | Actual analysis and process specification | Do not approve from carbon equivalent alone |
| Residual magnesium | Nodularization treatment indicator | Timed ladle analysis and treatment record | Bulk result does not prove local nodularity |
| Manganese | Pearlite and hardenability influence | Specified maximum/target and matrix report | Section response remains important |
| P, S and residuals | Embrittlement, treatment recovery and carbide risk | Full residual list and charge control | Generic typical values are not purchase limits |
Chemistry is a process input, not a finished-part guarantee
Nodularization, inoculation and pouring must be managed as a timed process. Treatment method, fade time, inoculant practice, stream control and pouring sequence should be appropriate to casting mass and wall range. Metallography from an agreed location provides a local observation; it should be interpreted together with mechanical tests, hardness mapping and section geometry.
Bulk heat analysis answers whether the sampled melt or bar conforms to ordered chemical limits. It cannot by itself prove local microstructure, discontinuity freedom, dimensional accuracy, surface condition, residual stress, magnetic response, fatigue resistance, corrosion resistance or service life. The control plan therefore has to connect chemistry with the ordered product form, manufacturing history, representative tests and final inspection.
| Interaction | Question for the engineer | Unsafe shortcut | Control evidence |
|---|---|---|---|
| C-Si + cooling rate | Will thin walls chill while bosses become more pearlitic? | One coupon represents every wall | Simulation/process review and location-specific checks |
| Mg + S/O | Is treatment recovery stable through the pour? | Passing one ladle number | Treatment timing, analysis and nodularity |
| Mn + section size | Can the matrix meet the agreed ferrite/pearlite target? | Inferring matrix from strength only | Metallography and hardness map |
| Geometry + feeding | Can bosses and flanges be fed without shrinkage? | Changing chemistry to cure all porosity | Gating/risering plan and NDT |
Bearing bores, split joints, dowels and oil passages
Bearing seats require more than a nominal diameter. The drawing should define datum hierarchy, roundness, cylindricity, coaxiality, surface texture and runout to the mounting face. For split housings, cap orientation, bolt condition, dowel relationship and line-boring state determine whether the measurement is meaningful.
Oil grooves, drain galleries, threaded ports and seal bores need core and machining definitions. Avoid thin residual walls behind a thread or abrupt junction between a heavy boss and light web. The supplier may propose a manufacturability change, but only the equipment engineer can approve its effect on stiffness, lubrication and assembly.
| Critical feature | Why it matters | Drawing/inspection input | Problem reduced |
|---|---|---|---|
| Bearing bore | Fit, alignment and heat generation | Diameter, form, coaxiality and texture | Fretting or premature bearing damage |
| Cap/base joint | Bore geometry under preload | Matched marking, dowels and torque condition | Assembly mismatch |
| Mounting feet | Shaft alignment | Flatness, height and datum relationship | Soft foot and distortion |
| Oil/seal features | Lubrication and leakage | Passage proof, bore finish and wall minimum | Blocked oil path or seal damage |

Pattern, sand mould, cores and feeding strategy
A sand-casting route may be proposed after reviewing size, quantity, surface and tolerance requirements. Pattern shrinkage, machining allowance, draft, parting, cores, chills, filters, risers and shakeout timing should be planned around the housing geometry. This page does not claim that every size can be produced by one moulding line.
Heavy bearing bosses connected to thin ribs create thermal gradients. Feeding and core support should be considered before tooling release; later machining cannot restore a shifted bore wall or remove internal shrinkage without violating the drawing. Repair welding, impregnation or inserts are not assumed and require written approval.
| Stage | Primary concern | Planned control | Traceable record |
|---|---|---|---|
| Tooling review | Wrong shrinkage/datum or inaccessible core | Drawing and process-design review | Tooling release record |
| Melt treatment | Fade, slag and inconsistent nucleation | Timed treatment and inoculation plan | Heat/ladle log |
| Mould/core assembly | Core shift and inclusions | Prints, chaplet policy and closure check | Mould traveler |
| Feeding/cooling | Shrinkage, carbide and distortion | Risers/chills and cooling rule | Pour and knockout record |
Matrix control, stress relief and property evidence
QT500-7 may be ordered in an as-cast or specified treated condition depending on the governing document and required matrix. Any ferritizing, normalizing or stress-relief cycle must be a qualified response to the actual section and machining plan. Furnace setpoint alone is not proof of part temperature or final structure.
If rough machining precedes stress relief, the sequence should preserve enough finishing stock and define dimensional reinspection. If no heat treatment is needed, that decision should still be recorded rather than inferred. Welding heat must not be introduced during fabrication or field repair without an approved ductile-iron procedure.
Section size, sampling and representation
Cast sample type, location and size influence reported tensile properties. Agree whether separately cast, side-by-side or attached samples are used, and identify metallographic and hardness locations on the actual housing. For a critical bearing boss, local hardness and structure can be more representative than an unrelated small coupon, while still not replacing design validation.
| Verification | Location or condition | Acceptance input | Limitation |
|---|---|---|---|
| Tensile test | Specified cast-sample condition | Grade values and method | Coupon-to-casting relationship is limited |
| Metallography | Named boss/wall or sample | Nodularity, graphite form and matrix criteria | Local field of view only |
| Hardness map | Bores, bosses, feet and walls | Locations and range | Hardness is not toughness |
| Stress relief | After rough machining if ordered | Cycle and dimensional recheck | Does not correct bad geometry |
Datum transfer, line boring and threaded features
Machine from casting datums transferred under a controlled setup plan. A split housing may need bolting, doweling and line boring as a matched assembly. Clamping must not force a distorted casting into nominal geometry that disappears after release.
Define rough and finish inspection stages, cutter access, burr removal, thread gauges and cleanliness of oil passages. Surface texture should be specified only where function requires it; an unnecessarily fine finish can add cost without correcting form error or bearing misalignment.
- Identify free-state and assembled-state dimensions.
- Protect matched cap/base identity through finishing.
- Specify bore, register, seal and mounting-face CTQs.
- Verify oil passages after machining and cleaning.
- Record thread gauge, deburring and insert rules.
- Preserve minimum wall after all cuts.

Inspection and quality-document package
The inspection plan should be risk-based. Visual and dimensional checks apply broadly; MT can address defined surface zones, while UT or RT applicability depends on geometry and agreed technique. No NDT method proves the absence of every discontinuity.
The dossier should link melt analysis, treatment records, test coupons, metallography, heat treatment, repair dispositions, dimensions and NDT to the casting identity. State document type and language in the purchase order rather than assuming a certificate format.
| Inspection layer | Purpose | Purchase-order definition | Method boundary |
|---|---|---|---|
| Chemistry/traceability | Grade and melt identity | Actual results and casting linkage | Does not prove local structure |
| Metallography/hardness | Nodularity and matrix outcome | Locations, method and acceptance | Sampled regions only |
| MT/UT/RT | Selected surface/internal zones | Technique, coverage and criteria | Geometry affects sensitivity |
| Dimensional report | Bearing and assembly CTQs | Datum, clamping state and sample plan | Inspection does not approve design |
Bore fretting, cap cracking, leakage and distortion analysis
Preserve the housing, matched cap, bearings, fasteners and lubricant evidence before cleaning. Bore fretting may arise from fit, preload, alignment, stiffness, surface finish or operating vibration. A crack may involve shrinkage, a sharp transition, assembly load, impact or unauthorized welding. Chemistry alone rarely identifies the mechanism.
A corrective action should follow evidence: dimensional mapping in free and clamped conditions, fracture origin, metallography, hardness, NDT, load history and lubrication review. Increasing strength or hardness without addressing geometry can move the failure elsewhere.
| Observed condition | Possible contributors | Evidence before a material change | Engineering boundary |
|---|---|---|---|
| Polished/fretted bore | Fit, cap preload, alignment or vibration | Bore form, fasteners, bearing and duty | OEM sets fit and preload |
| Crack at boss/web | Stress concentration, shrinkage or overload | Origin, section, NDT and loads | Do not change grade alone |
| Oil leakage | Porosity, crack, seal or passage | Leak map, NDT, wall and seal condition | Test condition must be approved |
| Mounting distortion | Residual stress, clamping or machining sequence | Free/clamped dimensions and route | Rework requires wall review |
Prototype, first-article and production release
The first order should be treated as a controlled industrialization exercise. Freeze the drawing revision, material specification, manufacturing route, witness points, deviation process and document index before production. A first article is useful only when its records remain linked to the same route that will be used for production; an unrecorded prototype is not a process qualification.
- Freeze drawing, assembly condition and CTQs.
- Confirm QT500-7 standard, edition and substitution policy.
- Approve pattern, cores, treatment and feeding plan.
- Link chemistry and treatment timing to castings.
- Complete agreed coupons, metallography and hardness.
- Review repair-prohibited zones and deviation route.
- Line-bore matched assemblies under the approved condition.
- Complete dimensional, NDT and cleanliness checks.
- Review first-article dossier before production release.
- Control every later process or source change.

Packaging, identification and change control
Protect machined bores, dowels, split faces, threads and oil openings with non-damaging covers and corrosion protection compatible with the buyer’s cleaning process. Keep matched caps and bases together, mark orientation and secure heavy housings against movement. Lifting points and center of gravity should follow the approved handling plan.
Marking must not damage a functional surface or erase traceability during finishing. Packaging should control corrosion, impact, contamination and movement in transit according to the actual component. Any proposed change to raw-material source, grade, product form, tooling, heat treatment, subcontract process, machining datum, inspection method or repair route should enter the agreed change-control process before shipment.
RFQ checklist for a QT500-7 bearing housing
A useful enquiry lets engineering compare the requested evidence with the actual risk. Send controlled files rather than relying on a photograph, trade name or sample alone. If a legacy component has failed, preserve the fracture, wear pattern, deposits and operating history before cleaning or sectioning.
- Controlled 2D drawing and 3D model with revision.
- Bearing arrangement, loads, speed, temperature and vibration.
- Free/clamped measurement and line-boring condition.
- QT500-7 governing standard and edition.
- Chemistry, residuals, nodularity and matrix criteria.
- Casting mass, wall range, tooling and annual quantity.
- Heat treatment or stress-relief requirements.
- Bore, foot, seal, thread and oil-passage CTQs.
- NDT method, zones, acceptance and sampling.
- MTC, marking, packing, destination and witness points.
Related products, material guidance and capability pages
QT500-7 material guide. ZG230-450 steel bearing housing comparison. Ductile iron piston and valve body. Materials. Engineering Resources. Quality Assurance. Factory Capability. Send Drawings for Quote.
This page targets a QT500-7 gearbox bearing-housing RFQ. The existing ZG230-450 steel bearing-housing product and general QT500-7 material guide retain different material or informational intent; the pages do not present those materials as interchangeable.
Current authoritative references
Standards are referenced to define questions and evidence, not to reproduce protected tables or claim automatic conformity. The purchase order must identify the required edition, grade, product form, supplements and acceptance criteria.
- ISO 1083:2018 spheroidal graphite cast irons.
- ASTM A536-26 ductile iron castings.
- ISO/TR 945-3:2016 cast-iron matrix structures.
- ISO 6892-1:2019 tensile testing at room temperature.
Engineering, commercial and safety boundary
This is a drawing-based manufacturing and RFQ page, not an online-retail listing, design approval or promise of stock, price, delivery time, service life, savings, certification scope or universal performance. The purchaser, equipment OEM and responsible engineer retain final responsibility for grade selection, chemistry limits, product form, loads, environment, corrosion or wear compatibility, dimensions, tolerances, heat treatment, joining, inspection, installation, lubrication, maintenance and retirement criteria. Final material, structure, thickness, dimensions and installation method must follow the customer-approved drawing and contract.
Melting, pouring, forging, heat treatment, machining, grinding, chemical analysis, magnetic testing, NDT, lifting and assembly can involve hot material, rotating machinery, fumes, dust, chemicals, electrical energy and heavy suspended loads. Qualified personnel, approved procedures, applicable law, guarding, ventilation, PPE, calibrated equipment and exclusion zones remain required. Existing site-library photographs provide product or process context only; their exact alloy, heat, customer and project provenance was not independently re-established and they do not prove conformity of a future order.