Description
Mill Rubber Lifter Bar
- Production Process: Sand Process
- Hardness: ≥ HRC60, BH310-380.
- Surface Finish: Appro.Ra100
- Size Tolerance: as per CT13
- Application: Chute Liners + Hopper Liners + Wear Plates
- Microstructure: Fine Martensitic + Carbonate + Retained Austenitic less than 5%
- Heat treatment Process: quenching & tempering treatment to achieve higher hardness and ideal impact value.
- Material Grade: AS 2074/L2A, AS2074/L2B, AS2074/L2C, ZG45Cr2Mo, ZG30Cr5Mo, ZG40Cr5Mo(FED-4A), ZG50Cr5Mo, FMU-29.
Our Photos for Mill Rubber Lifter Bar :
Chemistry Standard for Mill Rubber Lifter Bar
Standard Specification for Cr-Mo Alloy Steel: | |||||||||
Reference Standard | Nominal Chemical Composition (W%) | ||||||||
C | Si | Mn | P | S | Ni | Cr | Mo | ||
AS 2074/L2A | 0.45-0.55 | ≤0.75 | 0.50-1.00 | ≤0.04 | ≤0.04 | – | 0.80-1.20 | – | |
AS 2074/L2B | 0.55-0.65 | ≤0.75 | 0.50-1.00 | ≤0.04 | ≤0.04 | – | 0.80-1.50 | 0.2-0.4 | |
AS 2074/L2C | 0.70-0.90 | ≤0.75 | 0.50-1.20 | ≤0.04 | ≤0.04 | – | 1.30-2.40 | 0.2-0.4 | |
ZG42Cr2Si2MnMo | 0.38-0.48 | 1.5-1.8 | 0.8-1.2 | ≤0.04 | ≤0.04 | – | 1.8-2.2 | 0.2-0.6 | |
ZG45Cr2Mo | 0.40-0.48 | 0.8-1.2 | 0.4-1.0 | ≤0.04 | ≤0.04 | ≤0.5 | 1.7-2.0 | 0.8-1.2 | |
ZG30Cr5Mo | 0.25-0.35 | 0.4-1.0 | 0.5-1.2 | ≤0.04 | ≤0.04 | ≤0.5 | 4.0-6.0 | 0.2-0.8 | |
ZG40Cr5Mo(FED-4A) | 0.35-0.45 | 0.4-1.0 | 0.5-1.2 | ≤0.04 | ≤0.04 | ≤0.5 | 4.0-6.0 | 0.2-0.8 | |
ZG50Cr5Mo | 0.45-0.55 | 0.4-1.0 | 0.5-1.2 | ≤0.04 | ≤0.04 | ≤0.5 | 4.0-6.0 | 0.2-0.8 | |
ZG60Cr5Mo | 0.55-0.65 | 0.4-1.0 | 0.5-1.2 | ≤0.04 | ≤0.04 | ≤0.5 | 4.0-6.0 | 0.2-0.8 | |
FMU-29 | 0.25-0.45 | 0.3-1.0 | 0.6-1.5 | ≤0.04 | ≤0.04 | – | 6.0-8.0 | 0.2-0.4 | |
FMU-11 | 0.90-1.30 | 0.3-1.0 | 0.6-1.5 | ≤0.0 |