Description
EB Castworld accepts drawing-based enquiries for H62 Cu-Zn forged or wrought-stock worm gear blanks and machined gear rings. Candidate supply includes rough forged rings, saw-cut/turned blanks and finish-machined bronze-colored components before or after customer-approved tooth generation. Feasibility depends on section, stock route, gear geometry, load, lubricant, mating worm and inspection plan.
H62 is a Chinese wrought brass designation governed by the adopted edition of GB/T 5231. The current public national-standard record identifies GB/T 5231-2022 as the active standard for designations and chemical composition of wrought copper and copper alloys. H62 should not be described as a casting grade or automatically substituted with C28000, CuZn37 or another international designation without a controlled comparison.
Copper and zinc establish the brass system, while lead, iron and other residuals require limits. The designation does not guarantee one mechanical temper, machinability rating, dezincification resistance, tooth capacity or wear life. Product form, thermomechanical history, grain flow, stress relief, machining and application engineering remain part of the order.
Product scope and purchasing intent
The intended purchasing scope is a customer-defined blank or ring, not an off-the-shelf finished gearbox. State whether EB Castworld supplies only the blank, rough-turns datum surfaces, cuts teeth to an approved standard, or performs final inspection. The purchaser retains responsibility for gear rating, tooth geometry, contact pattern, lubrication, temperature, backlash and system safety.
Forging may be proposed for ring-shaped or stepped blanks when size, quantity and tooling justify it; approved wrought bar or plate routes may suit other parts. H62 chemistry belongs to wrought copper alloy. A sand-cast photograph or process cannot redefine it as a cast H62 product.
| Candidate supply | Required definition | Key risk | Approval boundary |
|---|---|---|---|
| Forged ring blank | OD/ID, faces, grain-flow intent and stock | Laps, eccentric stock and distortion | Gear designer approves blank envelope |
| Rough-machined hub blank | Datums, bore, hub and tooth allowance | Insufficient finishing stock | Purchaser defines tooth process |
| Machined gear ring | Module/DP, helix, quality and inspection | Wrong contact geometry | OEM owns gear rating |
| Legacy replacement | Authorized tooth data and mating-worm condition | Copying worn teeth | Purchaser approves recovered design |
H62 and current GB/T wrought-copper standards
GB/T 5231-2022 is the current Chinese national standard for designations and chemical composition of wrought copper and copper alloys. GB/T 4423-2020 is the current national standard for drawn copper and copper-alloy rod. Neither title by itself authorizes every forging, ring, mechanical temper or finished gear; the purchase order must identify the relevant product standard, state and test requirements.
ISO 1190-1:1982, confirmed current in 2024, explains a composition-based designation system for copper and copper alloys, but it is not an equivalence certificate for H62. ASTM B584-22 addresses copper-alloy sand castings and is cited only to emphasize that cast-product standards are separate from a wrought H62 order.
| Reference | Useful role | What it does not establish | RFQ instruction |
|---|---|---|---|
| H62 / GB/T 5231-2022 | Wrought alloy identity and chemistry | Finished gear properties | State edition and ordered product form |
| GB/T 4423-2020 | Drawn rod delivery context | Forged ring acceptance | Use only for matching bar supply |
| ISO 1190-1:1982 | Composition-based designation principles | Automatic H62 equivalence | Use as designation context only |
| ASTM B584-22 | Copper-alloy sand-casting scope | Authority to cast H62 | Do not apply to wrought H62 blanks |
Cu-Zn composition, residual elements and substitution control
Copper and zinc define the main alloy balance. The ordered standard controls actual limits and analytical rules; this page intentionally avoids converting a shorthand nominal percentage into a universal certificate range. Lead can strongly influence machinability and compliance, while iron and other residuals can influence structure, hot workability and surface behavior.
Request actual heat or batch analysis and define whether product analysis is required. If regulations restrict lead or other substances, provide the applicable jurisdiction, component category, exemption basis and analytical threshold. A generic ‘RoHS compliant’ statement is not a replacement for a contract-specific material declaration.
| Element/group | Metallurgical relevance | Evidence to request | Selection boundary |
|---|---|---|---|
| Copper | Base metal, conductivity and phase balance | Actual analysis to GB/T 5231 | Nominal name is not a test report |
| Zinc | Strength, phase balance and hot-working response | Calculated/reported balance and limits | More zinc changes corrosion and forming behavior |
| Lead | Machinability and regulatory concern | Specified limit and compliance evidence | Do not assume lead-free status |
| Fe and residuals | Structure, cleanliness and processing context | Full controlled-residual list | Typical supplier values are not universal |
Chemistry is a process input, not a finished-part guarantee
Composition interacts with billet quality, working temperature, reduction, cooling and final state. Overheating, insufficient working or unfavorable grain flow can create defects that a passing spectrometer result cannot reveal. If the blank is machined from bar rather than forged, the quotation and certificate should say so; process identity must not be blurred for marketing.
Bulk heat analysis answers whether the sampled melt or bar conforms to ordered chemical limits. It cannot by itself prove local microstructure, discontinuity freedom, dimensional accuracy, surface condition, residual stress, magnetic response, fatigue resistance, corrosion resistance or service life. The control plan therefore has to connect chemistry with the ordered product form, manufacturing history, representative tests and final inspection.
| Interaction | Question for the engineer | Unsafe shortcut | Control evidence |
|---|---|---|---|
| Cu/Zn + phase balance | Is the selected state suitable for hot working and service? | Approving from color | Analysis and product-form certificate |
| Pb/residuals + cutting | Can surface and burr requirements be met? | Calling every H62 heat equally machinable | Trial machining and limit review |
| Forging temperature + reduction | Will the ring be sound without laps? | Using chemistry to prove grain flow | Qualified route and macro/UT if ordered |
| Lubricant + environment | Is brass suitable for temperature and water chemistry? | Assuming universal corrosion resistance | OEM tribology and corrosion review |
Blank envelope, hub, rim and tooth-generation allowance
The blank drawing should separate finished gear geometry from supplier stock. Define bore, hub, web, rim, faces, keyway and tooth allowance relative to a common datum system. An eccentric ring can consume tooth stock on one side even if OD and ID each pass a simple two-point measurement.
Worm gearing creates sliding contact and heat. The gear engineer should define module or diametral pitch, pressure angle, lead/helix, hand, center distance, backlash, accuracy grade, surface finish and mating-worm material. H62 selection cannot replace a load and lubrication calculation.
| Critical feature | Why it matters | Drawing/inspection input | Problem reduced |
|---|---|---|---|
| Rim/tooth stock | Complete tooth depth and cleanup | Concentric allowance and minimum rim | Breakthrough or eccentric teeth |
| Hub and bore | Shaft fit and torque transfer | Fit, key/spline and runout | Fretting or misalignment |
| Web transition | Stiffness and forging flow | Radii, thickness and flatness | Crack or distortion |
| Datum faces | Setup and gear inspection | Primary/secondary datums and texture | Accumulated runout |

Billet qualification, ring forging and controlled cooling
Start with authenticated H62 wrought feedstock of appropriate size and condition. A forged-ring route can include billet cutting, heating, upsetting, punching, ring expansion or die forging, controlled cooling and descaling. The detailed route depends on blank size and equipment; no universal forging ratio or temperature is promised on this page.
Tooling and process review should address fold/lap risk, eccentric flow, end grain at the hub, oxide entrapment and enough stock for surface removal. Weld repair, plugging or brazed defect concealment is not assumed. Any repair route requires written purchaser approval and may be prohibited on tooth or hub regions.
| Stage | Primary concern | Planned control | Traceable record |
|---|---|---|---|
| Incoming billet | Wrong alloy or surface defects | MTC, identity and stock inspection | Receiving record |
| Heating | Zinc loss, oxidation or nonuniform temperature | Qualified window and furnace control | Heat log |
| Forging/ring forming | Laps, eccentricity and poor flow | Approved sequence and dimensions | Route traveler |
| Cooling/descale | Distortion, cracking and surface loss | Controlled handling and stock check | Post-forge report |
Material state, stress relief and representative testing
H62 blank properties depend on product form and material state. Hot-worked, annealed and cold-worked stock can respond differently during machining and service. The order should name the state required by the adopted product standard and the point at which mechanical tests apply.
A stress-relief treatment may be evaluated for a heavily machined or tight-tolerance ring, but it must be compatible with alloy, dimensions and final properties. The supplier should not invent a heat-treatment recipe merely to correct distortion after machining.
Section size, sampling and representation
A tensile specimen from feedstock or a separate test piece may not reproduce the rim, hub or worked transition. Define sample source and orientation, hardness locations and any macrostructure/ultrasonic examination required for heavy blanks. Gear-tooth performance still depends on final geometry, finish, contact and lubrication.
| Verification | Location or condition | Acceptance input | Limitation |
|---|---|---|---|
| Heat analysis | Feedstock heat/batch | GB/T chemistry limits | Not mechanical state |
| Tensile/hardness | Named stock or prolongation | State, orientation and method | Not gear capacity |
| Macrostructure/UT | Heavy ring zones if ordered | Technique and acceptance | Sensitivity depends on geometry |
| Stress relief | Defined route position | Qualified cycle and reinspection | Not a cure for folds |
Turning, bore control, keyways and tooth interfaces
Rough turn the OD, ID and faces from a stable datum strategy, leaving stock appropriate to later tooth generation and stress movement. Control chucking force so a thin ring is not accepted only while distorted in the fixture. Measure roundness and runout after release where function requires it.
Keyways, splines, threaded holes and lubrication features need edge, radius and position requirements. If EB Castworld is not contracted to cut teeth, the blank report should still verify the surfaces that the customer’s gear shop will use as setup datums.
- State whether dimensions apply free or clamped.
- Define concentric tooth stock around the datum bore.
- Control face parallelism and hub runout.
- Specify keyway or spline inspection method.
- Protect gear-cutting datum surfaces.
- Document all nonconformity dispositions before shipment.

Inspection and quality-document package
Certificate review, identity, visual condition and dimensions establish the incoming and finished blank. PT may be ordered on high-risk surfaces; UT applicability and acceptance depend on section and qualified technique. A final gear inspection, when in supply scope, should report the named quality standard and actual measured characteristics.
The dossier should link feedstock heat, forging lot, route, thermal records, inspection and deviations to each shipment. If chemical regulatory declarations are needed, keep them separate from mechanical certificates and identify the tested lot.
| Inspection layer | Purpose | Purchase-order definition | Method boundary |
|---|---|---|---|
| Chemistry/MTC | H62 identity and heat | Actual values, state and source | Does not prove forging soundness |
| Visual/PT | Surface laps and cracks | Stage, zones and criteria | Cannot prove internal soundness |
| Dimensions/runout | Usable tooth and hub stock | Datum, free state and CTQs | Does not approve gear design |
| Gear inspection | Tooth geometry when ordered | Standard, grade and report items | Contact/load validation remains OEM work |
Tooth wear, scoring, cracking and dezincification analysis
Preserve the gear, mating worm, lubricant and operating history. Tooth wear or scoring can involve load, alignment, lubrication, contamination, hardness, roughness or an unsuitable material pair. Rim cracking can involve geometry, forging laps, residual stress or shock. A copper-zinc chemistry result alone does not identify the root cause.
Dezincification or stress-corrosion concerns depend on environment, stress and alloy condition. Record water chemistry, temperature, cleaning agents and deposits before destructive examination. An alternate brass or bronze should be selected by the responsible tribology and corrosion engineer, not by color or a one-line equivalence chart.
| Observed condition | Possible contributors | Evidence before a material change | Engineering boundary |
|---|---|---|---|
| Scored tooth flank | Lubrication, debris, alignment or pairing | Contact pattern, oil, worm and roughness | OEM revises tribology |
| Uneven wear | Runout, lead error or deflection | Gear metrology and bearing alignment | Harder alloy may not fix geometry |
| Rim/hub crack | Lap, radius, interference or shock | Origin, macrostructure, fit and loads | Do not weld without approval |
| Selective corrosion | Fluid chemistry, stress and alloy state | Deposits, analysis and environment | H62 is not universally dezincification resistant |
Prototype, first-article and production release
The first order should be treated as a controlled industrialization exercise. Freeze the drawing revision, material specification, manufacturing route, witness points, deviation process and document index before production. A first article is useful only when its records remain linked to the same route that will be used for production; an unrecorded prototype is not a process qualification.
- Freeze blank and finished gear drawings.
- Confirm H62 standard, edition, form and state.
- Approve feedstock source and substitution rules.
- Review forging sequence and repair prohibition.
- Link chemistry and route to every lot.
- Inspect forged surfaces before machining.
- Verify free-state bore, faces and tooth stock.
- Complete ordered PT/UT and mechanical checks.
- Review first-article gear metrology if in scope.
- Control source, route and tooling changes.

Packaging, identification and change control
Protect finished bores, datum faces, keyways and any cut teeth with non-staining corrosion protection and rigid separators. Support rings to prevent ovalization and movement. Mark heat/lot and drawing revision on an approved nonfunctional location or durable tag; avoid steel-wire contact that can damage soft brass surfaces.
Marking must not damage a functional surface or erase traceability during finishing. Packaging should control corrosion, impact, contamination and movement in transit according to the actual component. Any proposed change to raw-material source, grade, product form, tooling, heat treatment, subcontract process, machining datum, inspection method or repair route should enter the agreed change-control process before shipment.
RFQ checklist for an H62 worm gear blank
A useful enquiry lets engineering compare the requested evidence with the actual risk. Send controlled files rather than relying on a photograph, trade name or sample alone. If a legacy component has failed, preserve the fracture, wear pattern, deposits and operating history before cleaning or sectioning.
- Controlled blank and finished-part drawings.
- Gear module/DP, lead, hand, quality and mating worm.
- Torque, speed, duty, temperature and shock load.
- Lubricant, contamination and corrosion environment.
- GB/T 5231 edition, H62 state and substitution rule.
- Feedstock form, forging route and grain-flow intent.
- Chemistry, lead/residual and regulatory requirements.
- Bore, hub, rim, face, keyway and stock CTQs.
- PT/UT, mechanical, dimensional and gear inspections.
- Quantity, marking, packing, destination and documents.
Related products, material guidance and capability pages
H62 brass material guide. H62 copper rod product. H62 brass plate product. Materials. Engineering Resources. Quality Assurance. Factory Capability. Send Drawings for Quote.
This page targets a transactional H62 worm-gear blank or ring RFQ. The existing H62 brass-rod Blog and copper-rod/brass-plate products retain informational or commodity-form intent; none is presented as automatic evidence of finished gear suitability.
Current authoritative references
Standards are referenced to define questions and evidence, not to reproduce protected tables or claim automatic conformity. The purchase order must identify the required edition, grade, product form, supplements and acceptance criteria.
- GB/T 5231-2022 current national-standard record.
- GB/T 4423-2020 drawn copper-alloy rod record.
- ISO 1190-1:1982 copper-alloy designation.
- ISO 6892-1:2019 tensile testing.
Engineering, commercial and safety boundary
This is a drawing-based manufacturing and RFQ page, not an online-retail listing, design approval or promise of stock, price, delivery time, service life, savings, certification scope or universal performance. The purchaser, equipment OEM and responsible engineer retain final responsibility for grade selection, chemistry limits, product form, loads, environment, corrosion or wear compatibility, dimensions, tolerances, heat treatment, joining, inspection, installation, lubrication, maintenance and retirement criteria. Final material, structure, thickness, dimensions and installation method must follow the customer-approved drawing and contract.
Melting, pouring, forging, heat treatment, machining, grinding, chemical analysis, magnetic testing, NDT, lifting and assembly can involve hot material, rotating machinery, fumes, dust, chemicals, electrical energy and heavy suspended loads. Qualified personnel, approved procedures, applicable law, guarding, ventilation, PPE, calibrated equipment and exclusion zones remain required. Existing site-library photographs provide product or process context only; their exact alloy, heat, customer and project provenance was not independently re-established and they do not prove conformity of a future order.